The Effect of Austenization and Isothermal Soaking Temperatures on the Wear of Perlite Steel
S. Kalaman, Handan Baycik, O. Aycan
article (Uluslararası, Hakemli) | Yazar(lar): S. Kalaman, Handan Baycik, O. Aycan | Yıl: 2020 | Dergi/Kurum: METAL SCIENCE AND HEAT TREATMENT | İndeks: WOS.SCI | DOI: 10.1007/s11041-020-00564-7 | Anahtar Kelimeler: perlite steel, isothermal transformation, interlamellar spacing, wear resistance — Özet: The authors have
The authors have studied grade R260 rail steel after austenization in the temperature range from 800 to 930 degrees C and isothermal soaking at 500, 550, and 600 degrees C followed by quenching in water. The steel structure and abrasive wear resistance were characterized. Recommendations concerning an increase in steel wear resistance were provided.